- Parametr
- Wartość
- Certification M1
- M1
- Certification O2
- O2
- Capacity (free foaming) (RB024)
- 43 - 48 l
- Capacity in gap (The value given for a gap with dimensions 35*1000*35 (width *length *depth [mm])) (RB024)
- 38 - 43 l
- Secondary increase in volume (post-expansion) (EN 17333-2:2020)
- 40 - 80 %
- Full cure time (RB024)
- 1,5 h
- Dimensional stability (EN 17333-2:2020)
- ≤ 5 %
- Flammability class (DIN 4102)
- B2
- Deformation at maximum shear force PN-EN 1607:2013
- ≥ 15 %
- Water absorbability after 24h at partial immersion PN-EN 1609:2013
- 1 kg/m³
- Dimensional stability, after 24h in temp. +40°C and in relative humidity in the length direction PN-EN 1604:2013
- +/- 3 %
- Dimensional stability, after 24h in temp. +40°C and in relative humidity in the width direction PN-EN 1604:2013
- +/- 3 %
- Dimensional stability, after 24h in temp. +40°C and in relative humidity in the thickness direction (direction of foam growth) PN-EN 1604:2013
- +/- 8 %
- Permanent deformation after compression up to 75% thickness (direction of foam growth) for 22 hours at + 35°C / 50% relative humidity, determined after 30 minutes of relaxation
- ≤ 25 %
- Permanent deformation after compression up to 75% thickness (direction of foam growth) for 22 hours at + 35°C / 50% relative humidity, determined after 1 minute of relaxation
- ≤ 23 %
- Permanent deformation after compression up to 75% thickness (direction of foam growth) for 22 hours at + 35°C / 50% relative humidity, determined after 1 hour of relaxation
- ≤ 22 %
- Permanent deformation after compression up to 75% thickness (direction of foam growth) for 22 hours at + 35°C / 50% relative humidity, determined after 24 hours of relaxation
- ≤ 15 %
- Tensile strength perpendicular for frontal surfaces (PN-EN 1607:2013-07)
- ≥ 50 kPa
- Deformation at maximum tensile force (PN-EN 1607:2013-07)
- ≥ 15 %
- Compressive strength (PN-EN 1607:2013-07)
- ≥ 30 kPa
- Compressive stress at 10% relative strain (PN EN 826:2013)
- ≥ 12 kPa
- Permanent deformation after compression to 75% thickness for 22 h, determined after 72 h of annealing [T=+35°C, RH=50%] (PN-EN ISO 1856:2018 method A)
- ≤ 10 %
- Adhesion of foam applied at -10°C to the substrate wood [PN-EN 1607:2013]
- ≥ 50 kPa
- Adhesion of foam applied at -10°C to the ALU substrate [PN-EN 1607:2013]
- ≥ 60 kPa
- Adhesion of foam applied at -10°C to PVC substrate [PN-EN 1607:2013]
- ≥ 60 kPa
- Adhesion of foam applied at -10°C to the concrete substrate (PN-EN 1607:2013)
- ≥ 50 kPa
- Adhesion of foam applied at -10°C to the substrate expanded clay concrete (PN-EN 1607:2013)
- ≥ 60 kPa
- Adhesion of foam applied at +35°C to the wood substrate [PN-EN 1607:2013]
- ≥ 50 kPa
- Adhesion of foam applied at +35°C to the aluminum substrate [PN-EN 1607:2013]
- ≥ 60 kPa
- Adhesion of foam applied at +35°C to PVC substrate [PN-EN 1607:2013]
- ≥ 60 kPa
- Adhesion of foam applied at +35°C to the concrete substrate (PN-EN 1607:2013)
- ≥ 30 kPa
- Adhesion of foam applied at +35°C to the substrate expanded clay concrete (PN-EN 1607:2013)
- ≥ 60 kPa
- Acoustic insulation (EN ISO 10140-1:2010+A1:2012+A2:2014)
- ≤ 62
- Heat conductivity coefficient (PN EN 12667:2002)
- 0,035
- Water vapour transmission coefficient (PN EN 12086:2013-07)
- 0,09
- Water vapor diffusion resistance coefficient (PN EN 12086:2013-07)
- 8
- Thermal resistance (after curing)
- -40 - +90 °C
- Orange
- +
- Can / applicator temperature (optimal +20°C)
- +5 - +35 °C
- Ambient/surface temperature
- -10 - +35 °C